Engineering stress uses the original cross-section, but a specimen gets thinner as it stretches. True stress uses the actual area and keeps rising until fracture. True strain adds up correctly over successive stretches, which makes it the standard for metal-forming simulations.
How to use the True Stress and True Strain Calculator
- Engineering strain ε
- Engineering stress σ
Results update as you type, every field has its own unit menu, and everything is calculated in your browser.
How it works
Enter the engineering strain (as a fraction) and engineering stress. Valid up to the onset of necking.
Inputs explained
| Field | What to enter |
|---|---|
| Engineering strain ε | A number |
| Engineering stress σ | Units: MPa, kPa, Pa, GPa, psi, ksi |
What each result means
- True strain = ln(1 + [Engineering strain ε])
- True stress = [Engineering stress σ]×(1 + [Engineering strain ε])
- Difference in strain = ([Engineering strain ε] – ln(1 + [Engineering strain ε]))÷[Engineering strain ε]×100
Example values
How the main result changes when Engineering strain ε changes and everything else stays at the example values above:
| Engineering strain ε | True strain |
|---|---|
| 0.075 | 0.0723 |
| 0.1125 | 0.1066 |
| 0.15 | 0.1398 |
| 0.1875 | 0.1719 |
| 0.225 | 0.2029 |
| 0.3 | 0.2624 |
Formula
ε_true = ln(1 + ε_eng), σ_true = σ_eng·(1 + ε_eng)
Worked example
Inputs: Engineering strain ε: 0.15; Engineering stress σ: 400 MPa.
Results: True strain = 0.139762; True stress = 460 MPa; Difference in strain = 6.825 %.
Key terms
- Necking
- Local narrowing of a specimen before fracture.
Frequently asked questions
Why is true stress higher than engineering stress?
The real cross-section shrinks as the specimen stretches.
When do the two strain measures differ?
Above a few percent strain.
Is the formula valid after necking?
No, because the deformation is no longer uniform.
Why is true strain additive?
ln(L₂/L₀) = ln(L₁/L₀) + ln(L₂/L₁).